Copper-tungsten alloy electrical contacts are key components in high-voltage circuit breakers, switchgear, isolating switches, and grounding switches. These copper-tungsten alloy contacts play a crucial role in "breaking and conducting" electrical currents. As one of the most important parts of electrical switches, copper-tungsten alloy electrical contacts are often considered the "heart" of the product.
Now, let's take a detailed look at "special high-conductivity copper-tungsten alloy electrical contact materials and their processing technology."
Reasons for Choosing Copper-Tungsten Alloy as Electrical Contact Material
Copper-tungsten alloy combines the advantages of both copper and tungsten, offering high strength, high density, high temperature resistance, arc erosion resistance, and excellent electrical and thermal conductivity. It also exhibits good machinability. By using high-quality tungsten powder and oxygen-free copper powder, and employing isostatic pressing (high-temperature sintering with copper infiltration), we ensure the product's purity and accurate composition, creating a fine microstructure with outstanding performance. The alloy features excellent arc-extinguishing properties, good electrical conductivity, efficient thermal conductivity, and low thermal expansion, making it an excellent choice for electrical contacts.

Special High-Conductivity Copper-Tungsten Alloy Electrical Contact Materials and Their Processing Technology
1.Special High-Conductivity Copper-Tungsten Alloy Electrical Contact Materials: Copper powder and tungsten powder.
2.Processing Technology for Special High-Conductivity Copper-Tungsten Alloy Electrical Contacts: (1) First, select copper powder and tungsten powder with suitable particle sizes and mix them in the correct proportions.
(2) Perform multiple cycles of heat treatment, pressing into shape, and crushing on the mixed raw powders. Then, proceed with isostatic pressing to form the desired shape and sinter them into copper-tungsten alloy billets.
(3) Finally, perform vacuum infiltration of the prepared copper with the sintered billets to ensure complete copper infiltration, producing special high-conductivity copper-tungsten alloy electrical contact materials with a porosity of less than 0.15%.
Key Considerations in the Processing of Special High-Conductivity Copper-Tungsten Alloy Electrical Contacts:
1.The heat treatment temperature is between 580–700°C, and the duration is 2–4 hours.
2.The pressing pressure for forming is between 4.5–8.5 tons/cm².
3.The copper powder used is passed through a 400 mesh sieve, and the tungsten powder particle size is between 3–6 μm.
4.The weight ratio of mixed copper powder to tungsten powder is 0.3–0.8:99.7–99.2.
5.The copper content in the electrical contact material produced using this process is 8–17%.
Applications of Special High-Conductivity Copper-Tungsten Alloy Electrical Contact Materials:
These materials are widely used in high-temperature-resistant materials, electrical alloys for high-voltage switches, electrical machining electrodes, microelectronic materials, and more.
Advantages of Special High-Conductivity Copper-Tungsten Alloy Electrical Contact Materials and Their Processing Technology:
1.The use of tungsten as the framework in the material results in high hardness and excellent wear resistance.
2.Due to the copper content, the electrical contacts exhibit improved performance in terms of current interruption, electrical conductivity, and current continuity. Additionally, the material maintains high performance consistency throughout its lifespan.
3.This contact material can be made into various shaped contacts, simplifying switchgear structures, eliminating the dispersion of springs in switches, and greatly improving component reliability.
4.Through innovative granulation processes and precise selection of process parameters, the distance between tungsten particles in the material is controlled, solving the difficulties of forming and infiltration, and no auxiliary flux is required during the sintering process.
5.Innovative processing ensures that copper completely infiltrates the billets during production, resulting in electrical contact materials with a porosity of less than 0.15%.
Example of Processing Special High-Conductivity Copper-Tungsten Alloy Electrical Contact Materials:
1.First, pass the copper powder through a 400 mesh sieve, and mix it with 3–6 μm tungsten powder in the weight ratio of 0.3–0.8:99.7–99.2.
2.Heat treat the mixed powders at 580–620°C for 2–4 hours, and press them into shape under a pressure of 4.5–8.5 tons/cm² and crush.
3.Perform a second heat treatment at 620–670°C for 2–4 hours, pressing and crushing under a pressure of 6–8.5 tons/cm².
4.Perform a third heat treatment at 670–700°C for 2–4 hours, pressing and crushing under a pressure of 6–8.5 tons/cm².
5.Finally, isostatically press the material into the desired shape, then sinter with spark discharge to form copper-tungsten alloy billets.
6.Perform vacuum infiltration on the prepared pure copper and the sintered billets to achieve 8–17% copper content, resulting in various shaped electrical contact materials with a porosity of less than 0.15%.
Factors Affecting Special High-Conductivity Copper-Tungsten Alloy Electrical Contact Materials:
1.Internal Factors:
(1) Structural Size: It is theoretically believed that the larger the contact's structural size, the stronger its ability to withstand arc erosion due to the energy being dissipated. However, due to the limitations of the switch structure, the contact size cannot be too large. Recently, research has led to the development of hollow contacts, insert-type contacts, or contacts with arc-extinguishing angles or rings. The aim is to allow the contact to dissipate heat faster after an arc is generated and maintain good contact even after erosion.
(2) Manufacturing Process: Currently, domestic manufacturers of copper-tungsten electrical contacts commonly use mixing, pressing, sintering, and infiltration methods. Some use pre-sintered tungsten frameworks, while others do not. In comparison, contacts made with pre-sintered tungsten frameworks typically show better performance than those made without it. In recent years, foreign manufacturers have adopted advanced techniques to improve the lifespan of electrical contacts, such as fiber reinforcement, isostatic pressing-impregnation, sintering-rolling, ion implantation, and arc melting methods. However, these new methods are still in the experimental stage in China.
(3) Tungsten Powder Particle Size: Studies show that both finer and coarser tungsten powders result in poor arc erosion resistance. The ideal approach is to mix fine and coarse tungsten powders in a certain ratio, but the mixture needs to be adjusted depending on the specific composition of the contact material (e.g., CuW50, CuW90). In practical production, tungsten powders of a wide range of sizes are often used to reduce process difficulty.
(4) Application Context: Research indicates that different contact materials are best suited to different environments. For example, in SF₆ circuit breakers, the ideal composition is Cu2030/W8070, while in air or vacuum switches, Cu10/W90 is preferred. In sleeve-type circuit breakers, Cu1520/W8580 is most resistant to erosion.
2.External Factors: Studies suggest that electrical currents with different characteristics lead to different transient behaviors, which in turn affect the erosion strength of the contacts. Once the contact material is selected, its electrical properties are fixed. The surrounding medium has a significant effect on the arc-extinguishing ability of the electrical contact. For instance, a medium with strong arc-extinguishing properties greatly reduces arc erosion damage (which is a primary cause of point contact failure). In medium- and low-voltage switches, air or vacuum is commonly used as the arc-extinguishing medium, while in medium- and high-voltage circuit breakers, oil or SF₆ is used for this purpose. Additionally, the switching speed and initial pressure during the contact's opening and closing significantly influence its performance. Faster opening speeds, especially the initial opening speed, reduce the arc duration and minimize damage. Increasing the initial pressure reduces mechanical vibration caused by impact, thereby decreasing mechanical wear and arc erosion.