I. Selection of Welding Materials and Equipment
The proper selection of welding wire is fundamental to ensuring welding quality. In titanium tube welding, ERTi-2 welding wire should be given priority. ERTi-2 welding wire has good compatibility with the titanium tube base material, enabling the formation of a uniform and dense weld structure during welding, ensuring that the mechanical properties and corrosion resistance of the weld joint are similar to those of the base material. 2. Shielding Gas The shielding gas plays a crucial role in the welding quality of titanium tubes. Titanium readily reacts with oxygen and nitrogen in the air at high temperatures, forming brittle compounds that reduce the performance of the weld. Therefore, high-purity argon must be used as the shielding gas, with a purity ≥99.995% and a water content ≤50mg/m³. High-purity argon provides continuous and effective protection to the molten pool and high-temperature zone, preventing titanium from reacting with harmful gases in the air. 3. Welding Method Considering the low thermal conductivity of titanium, manual tungsten inert gas (TIG) welding is recommended. Manual tungsten inert gas (TIG) welding offers advantages such as stable arc, concentrated heat, and minimal welding deformation. It allows for precise control of welding heat input, meeting the requirements of titanium tube welding. Furthermore, this welding method facilitates operator observation of the molten pool, enabling timely adjustments to welding parameters and ensuring weld quality.
II. Careful Pre-Welding Preparation:
The quality of the bevel directly affects the performance of the weld joint. An alumina grinding wheel should be used to grind the bevel. During grinding, care must be taken to control the force and speed to avoid overheating and discoloration of the base material. Overheating leads to coarse grains in the base material, reducing its mechanical properties. The bevel shape must be smooth. The inner and outer surfaces within a 50mm radius should be ground and polished to remove surface oxide scale, oil, and other impurities. Then, clean with acetone to ensure a clean bevel surface. Cleaning Management: Titanium tube welding requires extremely high cleanliness. If the bevel and welding wire are left for more than 2 hours, the surface may absorb dust, moisture, and other impurities from the air, requiring re-cleaning. Self-adhesive tape can also be used to seal and protect the bevel and welding wire from contamination. Operators must wear clean gloves during the operation to prevent oil from their hands from contaminating the surface of the workpiece.
III. Strictly Adhere to Welding Process Specifications and Parameter Control:
During welding, low heat input welding should be used, i.e., low current and slow welding speed. This reduces the heat input, shrinks the heat-affected zone, and decreases the degree of grain coarsening in the heat-affected zone. Simultaneously, the interpass temperature must be strictly controlled, and should be ≤200℃. Excessively high interpass temperatures will lead to grain coarsening and reduce the mechanical properties of the weld. Argon Protection Measures: Different argon protection measures should be adopted for titanium pipes of different diameters. For large-diameter titanium pipes, personnel inside the pipe must wear respirators and hold protective shields to cover the back of the molten pool for localized protection. For small-diameter or fixed-end titanium pipes, a whole-pipe argon purging method should be used. Seal the inside of the pipe 150-300mm from the bevel with soluble paper, then purge the pipe with argon, ensuring the molten pool and high-temperature zone are in a good argon protective atmosphere. Operational Details: During welding, it is forbidden to strike an arc on the surface of the workpiece to avoid arc scratches, which will affect the appearance and quality of the weld. After the arc is extinguished, the welding wire must be removed under argon protection to prevent oxidation of the wire tip. Argon purging should be delayed after arc interruption until the workpiece temperature drops below 300℃ to prevent oxidation from contact with air at high temperatures.
IV. Quality Inspection and Defect Control Weld Color Analysis:
Weld color is an important and intuitive indicator of welding quality. A silvery-white weld indicates good argon protection during welding, that the weld has not been oxidized, and that the quality is acceptable. Blue or yellow welds indicate oxidation contamination, which may affect the weld's mechanical properties and corrosion resistance, requiring rework. Non-Destructive Testing: Non-destructive testing is a crucial means of ensuring welding quality. Penetrant testing should be performed on the root weld to detect defects such as cracks and porosity on the weld surface. X-ray testing should be performed on the entire weld to check for internal defects such as cracks, porosity, and lack of fusion, ensuring that the weld quality meets relevant standards. Mechanical Property Testing: The protective effect is evaluated using pickling. The changes in the weld surface after pickling are observed to determine the effectiveness of argon protection during welding. Meanwhile, tensile strength and plasticity tests were conducted on the welded joints to verify whether the mechanical properties of the weld met the design requirements.
V. Technological Innovation and Structural Optimization
The composite pipe welding technology adopts a patented titanium-steel composite pipe design, combining the titanium and steel layers through a special process. During welding, reasonable welding process parameters and welding sequence can improve welding strength and sealing performance, fully leveraging the advantages of both titanium and steel to meet the requirements of different working conditions. The protective device has been improved by adopting a full copper protective cover. The full copper protective cover has excellent thermal conductivity and chemical stability, reducing iron ion contamination and preventing iron ions from reacting with titanium to form brittle compounds. Simultaneously, the full copper protective cover better adapts to all-position welding requirements, improving welding quality and efficiency. The processing and welding technology of titanium pipes requires strict control at every stage, from the selection of welding materials and equipment, pre-welding preparation, welding process specifications, quality inspection to technological innovation and structural optimization; each step is crucial. Only by strictly adhering to technical requirements can the welding quality of titanium pipes be guaranteed, ensuring their safe and reliable application in various fields.